pubmed:abstractText
Increasingly higher concentrations of Phenyl-P in 30% HEMA were used as dentin conditioners to improve the bonding of adhesive resins to smear layers. The maximum bond strength (10.4 MPa) was obtained at a concentration of 20% Phenyl-P. Transmission electron microscopy of fractured, lightly smeared, and compactly smeared dentin demonstrated that 20% Phenyl-P in 30% HEMA demineralized the dentin surface by partially dissolving mineral crystals from around collagen. When applied to smear layers, this resin system demineralized the smear layer and incorporated it into the applied resin which penetrated a short distance into the underlying dentin, thereby creating a hybrid layer that contained the original smear layer. This single-step conditioner/primer offers several advantages over previous bonding systems by permitting a single solution to serve as both a conditioner and a primer.
pubmed:grant
pubmed:language
eng
pubmed:journal
pubmed:citationSubset
D
pubmed:chemical
pubmed:status
MEDLINE
pubmed:month
Jun
pubmed:issn
0022-0345
pubmed:author
pubmed:issnType
Print
pubmed:volume
73
pubmed:owner
NLM
pubmed:authorsComplete
Y
pubmed:pagination
1212-20
pubmed:dateRevised
2007-11-14
pubmed:meshHeading
pubmed:year
1994
pubmed:articleTitle
Bonding to ground dentin by a phenyl-P self-etching primer.
pubmed:affiliation
Division of Organic Materials, Tokyo Medical and Dental University, Japan.
pubmed:publicationType
Journal Article, Research Support, U.S. Gov't, P.H.S.