pubmed:abstractText
Silica-clad optical fibers comprising a core of crystalline germanium were drawn using a molten core technique. With respect to previous fibers drawn using a borosilicate cladding, the present fibers exhibit negligible oxygen despite being fabricated at more than twice the melting point of the germanium. The counterintuitive result of less oxygen when the fiber is drawn at a higher temperatures is discussed. The measured propagation loss for the fiber was 0.7?dB/cm at 3.39??m, which is the lowest loss reported to date.
pubmed:language
eng
pubmed:journal
pubmed:status
PubMed-not-MEDLINE
pubmed:month
Mar
pubmed:issn
1539-4794
pubmed:author
pubmed:issnType
Electronic
pubmed:day
1
pubmed:volume
36
pubmed:owner
NLM
pubmed:authorsComplete
Y
pubmed:pagination
687-8
pubmed:year
2011
pubmed:articleTitle
Silica-clad crystalline germanium core optical fibers.
pubmed:affiliation
The Center for Optical Materials Science and Engineering Technologies (COMSET), School of Materials Science and Engineering, Clemson University, Clemson, South Carolina 29634, USA. jballat@clemson.edu