The thermoelectric performance of EuZn(2)Sb(2) and EuCd(2)Sb(2) was optimized by mixed occupation of the transition metal position. Samples in the solid solution Eu(Zn(1-x)Cd(x))(2)Sb(2) with the CaAl(2)Si(2)-type crystal structure (space group Pm1) were prepared from the elements for compositions with x = 0, 0.1, 0.3, 0.5 and 1. The thermoelectric properties were investigated after densification of the products by spark plasma sintering (SPS). The samples show low electrical resistivity, high thermopower and a low lattice thermoconductivity. The highest ZT value of 1.06 at 650 K is obtained for x = 0.1.
|
pubmed:language |
eng
|
pubmed:journal | |
pubmed:status |
PubMed-not-MEDLINE
|
pubmed:month |
Jan
|
pubmed:issn |
1477-9234
|
pubmed:author | |
pubmed:issnType |
Electronic
|
pubmed:day |
28
|
pubmed:volume |
39
|
pubmed:owner |
NLM
|
pubmed:authorsComplete |
Y
|
pubmed:pagination |
1101-4
|
pubmed:year |
2010
|
pubmed:articleTitle |
Thermoelectric properties of Eu(Zn(1-x)Cd(x))2Sb2.
|