pubmed:abstractText |
For the purpose of finding out the method which is able to evaluate nonprecious metal/porcelain bond strength easily, Ceramco procelain was fused to casted Wiron "S" (3 mm diameter), by means of 5 types of press condensing methods; the bond strength was measured by pull out method and these condensing methods were compared. Results are follows: (1) No significant difference was observed between conventional condensing method and press condensing method (condensing pressure; 472-1 415 kg/cm2), and the bond strength of Ceramco Paint-O-Pake porcelain to Wiron "S" was about 245-369 kg/cm2. (2) Bond strength was decreased with the decrease of the fused length of procelain. (3) Bond strength was increased approximately three times, when specimens were mounted by dental stone.
|
pubmed:language |
jpn
|
pubmed:journal | |
pubmed:citationSubset |
D
|
pubmed:chemical | |
pubmed:status |
MEDLINE
|
pubmed:month |
May
|
pubmed:issn |
0583-0273
|
pubmed:author | |
pubmed:issnType |
Print
|
pubmed:volume |
17
|
pubmed:owner |
NLM
|
pubmed:authorsComplete |
Y
|
pubmed:pagination |
112-9
|
pubmed:dateRevised |
2009-11-11
|
pubmed:meshHeading | |
pubmed:year |
1976
|
pubmed:articleTitle |
[Bond strength between nonprecious metal alloy and porcelain. Part (1). Bond strength with press condensing method (author's transl)].
|