pubmed-article:10509330 | pubmed:abstractText | This in-vitro study evaluated shear bond strength and analyzed, via scanning electron microscopy, enamel prepared for pit and fissure sealant placement. Various surface pretreatment methods were conducted prior to short-term (72-hour) and long-term (120-day) analysis. | lld:pubmed |